Kim and Withey discuss the formation of an ‘intermediate layer’, formed between grains, which they observe in some Ni-base superalloys. This author proposes that the layer is the result of the presence of a bifilm, a double film probably of oxide or nitride, which appears to be capable of providing a coherent explanation of all the interesting observations reported by the authors.

 